Paint is an important part of interior decoration. It is prone to some thorny problems and people are helpless. In fact, as long as you identify the real cause of the problem, it is not difficult to have satisfactory results for the remedy. The supervision company's experts come to solve the problem for you to find a solution.
Paint peeling
It may be because the surface is too smooth. If the original paint is lacquer or powder (with untreated sizing paint), the new paint will not stick to the surface. Or it may be wood decay or metal rust, or peeling off due to poor paint quality. A small area of ​​paint is peeling off. It can be sanded with fine sandpaper, then putty put on it, brushed with a primer and repainted. Exfoliation over a large area must scrape all the paint off and repaint it.
Paint foaming
First of all, the puncture is broken. If there is water coming out, it means that under the lacquer layer there is moisture infiltration underneath or behind it. After the sun shines and the water evaporates into vapor, the paint is lifted up into foam. At this point, the blistering paint is removed with a hot air gun, the wood is allowed to dry naturally, then the primer is applied, and finally the entire repair surface is repainted. If there is no water in the bubble, it may be cracked wood grain, there is a small amount of air, the sun through the sun, the air expands, the paint bulge.
Faced with this situation, first scrape off the blistering paint, then use a resin filler to fill the cracks, repaint it, or use no filler. After the paint is peeled off, apply a microporous paint directly.
Cracked
In most cases, the paint must be removed with a chemical paint remover or a hot air gun and then repainted. If the fracture range is not large, then sanding blocks or wet or dry sandpaper can be used to dilute the broken paint. After the surface has been smoothed, apply putty, apply a primer, and repaint it.
Paint flow
Once the paint is too thick, it will cause runny. The paint can not be dry yet. Brush it with a brush. If the paint has started to dry, dry it. Use a fine sandpaper to smooth the paint, clean the surface, clean it with a damp cloth, and re-apply it. Outer paint, be careful not to brush too thick.
Stain
There are many causes of stain on the paint surface. For example, the moisture in the latex paint dissolves the substance on the wall and the paint surface is rusted. The wall surface that is rubbed with the steel wool will cause rust spots, and the dark pipe inside the wall will appear with stains.
In order to prevent stains, a layer of primer containing aluminum powder may be applied first. If stains are present, remove the emulsion paint at the stains first, brush the primer layer containing aluminum powder, and then re-paint.
Three trees paint paint latex paint interior decoration
PVC High Speed Door are designed for indoor use and ensure rapid handling operations between different areas that should remain separated. These safe and efficient industrial doors are made of a shaped steel frame and covered with PVC. These high speed doors are safe and efficient and consist of a shaped steel frame covered with PVC. Safety is ensured by their photocells and barriers.
High speed doors protect us from harm, save energy and help us to separate processes for optimal productivity. A high speed door's most important job is to simply open and close quickly and safely every time you need it.
The high speed pvc roll shutter door require high strains, caused by the high operating speed and the frequency of openings, have to be taken into account during construction. In the same way, basic conditions like size and installation location add up to considerable requirements regarding safety and control technique.
PVC High Speed Door,Large PVC High Speed Door,Transparent High Speed Door,Great Performance High Speed Door
Shenzhen Hongfa Automatic Door Co., Ltd. , https://www.spiralfastdoor.com